Textured yarns
Raw-white untwisted: tex 5,5 f 32, 7,6 f 32, 8,3 f32, 9,2 f 32, 12 f 32, 16 f 48, 16,7 f48, 18,5 f 48
Raw-white air-entangled: tex 9,2 f 32, 12 f 32, 16 f 48, 16,7 f48, 18,4 f64, 18,5 f 48, 22,2 f 64, 24,5 f 64, 33,4 f 96, 37,2 f 96
Raw-white twisted: tex 25 f 64, 33,4 f 96, 37,5 f 96
Dyed untwisted: tex 8,5 f 32, 9,3 f 32, 12,5 f 32, 16,3 f 48, 17 f 48, 18,8 f 48
Dyed air-entangled: tex15,5 f 64, 19 f 48, 25,4 f 64, 38,5 f 96
Dyed twisted: tex25,4 f 64, 38,2 f 96
For carpets and textile haberdashery raw white: 18,5 tex, 34 tex, 37,0 f 96 è f 128, 36 tex, 48,7 tex, 25 f 64, 27 f 96, 37 f 96, 48 f 144
For carpets and textile haberdashery dyed: 18,8 tex f 64, 25,4 tex f 64, 37 tex f 96, 38,2 tex, 48,7 tex
Physical properties
Qualitative cgaracteristics* | Raw white |
Air-entangled TP RB 400031289.190-2003 |
Dyed | For carpets and textile haberdashery | ||
---|---|---|---|---|---|---|
Untwisted | Twisted | Raw white | Dyed | Untwisted and Twisted | Raw white and Dyed | |
Unit breaking load, mN/tex, min | 290 | 290 | 280 | 280 | 290 | 280 |
Elongation at break, % | 24 ±5 | 25 ± 5 | 24 ± 4 | 24 ± 5 | 25±5 | 24±5 |
Variation coefficient in elongation at break, %, max | 12 | 13 | 13 | 13 | 13 | - |
Deviation of actual linear density from nominal one, %, max | ±2,0 | ± 2,5 | ± 2,5 | ± 2,5 |
+2 -3 |
+2,5 |
Variation coefficient in linear density, %, max | 2,5 | 2,5 | - | - | - | - |
Degree of crimp — for 12 tex — for 9,2 tex |
16±3 26±3 20±3 |
14±3 | - | - | 3,5-7,5 | - |
Crimp stability, % min | 65 | 63 | - | - | 55 | - |
Number of knots per 1 m, min | - | - | 100 | 100 | - | - |
Oil content, % | 0,8–3,8 | 0,8–3,8 | 0,7–4 | 0,7–4 | 0,8–3,8 | 1–4 |
Number of twists per 1 m | 65±10; 120±10 | - | - | 60±10, 120±10 | 65±10; 40±10 | |
Linear shrinkage, % | 6 | 6 | 6 | - | - | - |
Bobbin weight, g for tex 9,3 12,5 and 38,2 for tex 18,8 and 25,4 |
2800±200 - - |
2500±200 2200±200(120 TPM) - |
2500±200 - - |
2400±200 - - |
- 2300±200 2400±200 |
2500±300 |
Characteristics are indicated: for raw white yarn — grade «A», for dyed yarns — grade «b».
Polyester yarns are produced on cross-wound polypropylene cylindrical tubes.
Application: production of various textiles: lining, apparel textiles, furniture fabrics, jacquard fabrics, fabrics for automotive industry, gobelins, technical fabrics, awning fabrics, stockinet cloths, hosiery, fabrics for haberdashery: hangings and laces, gloves, carpets, ropes, tapes, basis for artificial fur, needlepunched materials and so on.
Packing: in carton boxes (760×380×304 mm), 8 bobbins per box.